CHEMONIL REDU electroless nickel
Middle phosphorus content (8-10 %)
CHEMONIL REDU 810
Fast electroless process depositing adherent, thick, pore-free and extremely wear and corrosion resistant nickel layers. It is based on nickel chloride, thus not applicable in stainless steel tanks. It produces closed pore-free layers already hence 4 µm.
High phosphorus content (10-12 %)
CHEMONIL REDU 812 and CHEMONIL REDU 812 (lead-free)
Fast electroless process depositing adherent, thick, pore-free and extremely wear and corrosion resistant nickel layers. It is based on nickel sulphate and complies with ROHS –and ELV.
The innovative stabilizer system allows Litre loads of 0.1 - > 2.0 dm2/L and cost savings by lower operation temperatures (80 – 88°C) in comparison to conventional systems.
The deposition rate lies in the range of 10 –14 μm per hour at a service life time of over 6 MTO.